| GROUP I Film defects | GROUP II Explanation |
|---|---|
| (P) Orange peel effect | (1) Inadequate spreading of the coating solution before Drying causes a bumping effect on the coating |
| (Q) Blistering | (2) It is the result of drying coated tablets in ovens, due to too Rapid evaporation of the solvent from the core and the Effect of high temperature on the film |
| (R) Cracking | (3) Occurs due to processing temperature used is too high for Aparticular formulation |
| (S) Bloom | (4) Occurs if internal stress in the film exceed the tensile Strength of the film |